I will love to go for a bond if the following is well taken care of:
Good salary with provision for annual or biannual upward review
If the working environment is satisfactory
If the job will enhance my professionalism
If the safety records of the company is good
If the company have a chance of...
Yes you can use a crushed aggregate sand for concrete, but you need to embark on a trial mix to check the effect on water demand and strength,since the dust con/fine content is higher with crushed stone sand, and of course you will need to increase your cement content to cope with increase...
Most likely caused by slow hydration resulting from overdosage of water reducing/ plasticising admixture.That it is only the column base that is affected, is that the the mix of the admixture was not homogeneous.
What you call standard in your place may not be standard in another.For you to know or determine the volume of your head pan and wheelbarrow,you will have to fill in them a measured amount of water. If the water required to fill your headpan is 25 litres, and amount of water filling your wheel...
Asking of chemical admixtures, we have the water reducing, plasticising, water-reducing/plasticising ,waterproofing, superplasticising/water reducing, air -entrainment , accelerating and retarding admixtures etc. There are many more, depending on what you want to achieve.
You will have to carry out non destructive tests,such as rebound hammer, and if the client argues that the rebound hammer will show only the surface hardness, you go ahead to do pulse velocity or coring.But note that in coring,there is no universally accepted means of interpreting the...