Details about building not given.
May be due Plumbing issues if there is toilet at that location.
The defect in plumbing system and then suitable waterproofing can work
Also sand quality (fineness / too fine) can be another reason for these sort of patches, Also presence of salt in water / sand used for plastering can also be a reason for this failure